family
Thymelaeaceae
The family Thymelaeaceae supplies 3 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
1 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Burn noseDaphnopsis americana | 479 lbf* | 27.5 lb/ft³ |
| RaminGonystylus bancanus | 1,300 lbf | 39.6 lb/ft³ |
| Variableleaf false oheloWikstroemia sandwicensis | 1,007 lbf* | 38.8 lb/ft³ |