Wood Record

family

Tiliaceae

The family Tiliaceae supplies 5 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

5 of 5 carry a published Janka test.

WoodJankaDensity
Açoita-cavaloLueheopsis duckeana1,767 lbf48.9 lb/ft³
DuruApeiba spp.250 lbf14.0 lb/ft³
EstribeiroLuehea spp.900 lbf38.0 lb/ft³
Pau-de-jangadaApeiba echinata558 lbf26.7 lb/ft³
ThitkaPentace spp.1,118 lbf40.0 lb/ft³