Wood Record

family

Ulmaceae

The family Ulmaceae supplies 14 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

4 of 14 carry a published Janka test.

WoodJankaDensity
African CeltisCeltis spp.1,670 lbf45.0 lb/ft³
American elmUlmus americana830 lbf35.0 lb/ft³
Cedar elmUlmus crassifolia1,419 lbf*45.5 lb/ft³
Chinese elmUlmus parvifolia1,152 lbf*41.3 lb/ft³
English elmUlmus procera1,152 lbf*41.3 lb/ft³
Japanese elmUlmus davidiana1,152 lbf*41.3 lb/ft³
Japanese zelkovaZelkova serrata1,725 lbf*49.9 lb/ft³
PlanertreePlanera aquatica1,054 lbf*39.6 lb/ft³
Rock elmUlmus thomasii1,320 lbf44.1 lb/ft³
San Domingo-BoxwoodPhyllostylon brasiliensis2,692 lbf*59.0 lb/ft³
September elmUlmus serotina1,152 lbf*41.3 lb/ft³
Siberian elmUlmus pumila1,152 lbf*41.3 lb/ft³
Slippery elmUlmus rubra860 lbf37.1 lb/ft³
Winged elmUlmus alata1,475 lbf*46.4 lb/ft³