Wood Record

family

Urticaceae

The family Urticaceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 6 carry a published Janka test.

WoodJankaDensity
FlameberryUrera caracasana369 lbf*24.3 lb/ft³
PumpwoodCecropia schreberiana298 lbf*22.0 lb/ft³
ScratchbushUrera baccifera197 lbf*18.2 lb/ft³
SogaPipturus argenteus451 lbf*26.7 lb/ft³
Trumpet treeCecropia obtusifolia321 lbf*22.8 lb/ft³
Waimea pipturusPipturus albidus369 lbf*24.3 lb/ft³