The family Verbenaceae supplies 7 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

5 of 7 carry a published Janka test.

WoodJankaDensity
FiddlewoodVitex spp.1,160 lbf43.0 lb/ft³
GmelinaGmelina arborea622 lbf30.0 lb/ft³
Golden dewdropsDuranta erecta1,103 lbf*40.5 lb/ft³
MolaveVitex spp.1,255 lbf50.0 lb/ft³
Spiny fiddlewoodCitharexylum spinosum1,598 lbf*48.1 lb/ft³
TeakTectona grandis1,000 lbf40.0 lb/ft³
VitexVitex doniana680 lbf29.8 lb/ft³