Wood Record

family

Viburnaceae

The family Viburnaceae supplies 5 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 5 carry a published Janka test.

WoodJankaDensity
BlackhawViburnum prunifolium1,923 lbf*52.4 lb/ft³
Common elderberrySambucus nigra832 lbf*35.5 lb/ft³
NannyberryViburnum lentago1,658 lbf*48.9 lb/ft³
Red elderberrySambucus racemosa672 lbf*32.2 lb/ft³
Siebold's arrowwoodViburnum sieboldii1,538 lbf*47.3 lb/ft³