Wood Record

family

Vochysiaceae

The family Vochysiaceae supplies 10 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

8 of 10 carry a published Janka test.

WoodJankaDensity
CedrinhoErisma uncinatum874 lbf35.5 lb/ft³
MandioqueiraRuizterania albiflora = Qualea albiflora1,351 lbf42.0 lb/ft³
MandioqueiraQualea gracilior = Qualea cf lancifolia1,071 lbf44.7 lb/ft³
MandioqueiraQualea brevipedicellata2,165 lbf58.7 lb/ft³
Mandioqueira-escamosaQualea dinizii1,363 lbf*44.7 lb/ft³
QuarubaVochysia guianensis1,427 lbf40.1 lb/ft³
QuarubaVochysia maxima976 lbf36.0 lb/ft³
QuarubaVochysia obidensis1,179 lbf38.0 lb/ft³
QuarubaVochysia ferruginea608 lbf*30.0 lb/ft³
YemeriVochysia spp.605 lbf36.0 lb/ft³