family
Zygophyllaceae
The family Zygophyllaceae supplies 4 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
1 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| HolywoodGuaiacum sanctum | 5,728 lbf* | 87.1 lb/ft³ |
| Lignum-vitaeGuaiacum officinale | 5,728 lbf* | 87.1 lb/ft³ |
| LignumvitaeGuaiacum spp. | 4,500 lbf | 80.0 lb/ft³ |
| VerawoodBulnesia arborea | 5,180 lbf* | 78.0 lb/ft³ |