7 of 11 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Balsam firAbies balsamea | 380 lbf | 24.5 lb/ft³ |
| California red firAbies magnifica | 500 lbf | 26.6 lb/ft³ |
| Fraser firAbies fraseri | 449 lbf* | 26.7 lb/ft³ |
| Grand firAbies grandis | 490 lbf | 25.8 lb/ft³ |
| Noble firAbies procera | 410 lbf | 27.3 lb/ft³ |
| Pacific silver firAbies amabilis | 430 lbf | 30.1 lb/ft³ |
| Santa Lucia or bristlecone firAbies bracteata | 449 lbf* | 26.7 lb/ft³ |
| Shasta red firAbies shastensis | 449 lbf* | 26.7 lb/ft³ |
| Silver firAbies alba | 576 lbf* | 31.5 lb/ft³ |
| Subalpine firAbies lasiocarpa | 350 lbf | 22.3 lb/ft³ |
| White firAbies concolor | 480 lbf | 27.3 lb/ft³ |