WoodJankaDensity
AuriAcacia auriculiformis1,598 lbf*48.1 lb/ft³
Australian BlackwoodAcacia melanoxylon1,100 lbf40.0 lb/ft³
Black wattleAcacia mangium1,007 lbf*38.8 lb/ft³
Black wattleAcacia mearnsii1,990 lbf*53.3 lb/ft³
Black WattleAcacia mollissima1,750 lbf45.0 lb/ft³
Green wattleAcacia decurrens1,054 lbf*39.6 lb/ft³
KoaAcacia koa2,287 lbf*56.9 lb/ft³
MulgaAcacia aneura3,749 lbf*71.5 lb/ft³
Prickly MosesAcacia verticillata1,054 lbf*39.6 lb/ft³
Silver wattleAcacia dealbata1,054 lbf*39.6 lb/ft³
Small Philippine acaciaAcacia confusa2,367 lbf*57.7 lb/ft³
Sydney golden wattleAcacia longifolia1,538 lbf*47.3 lb/ft³