genus
Aesculus
Woods sold under several trade names often come from one genus. These 7 share the genus Aesculus, so they are close relatives and frequent substitutes for each other.
0 of 7 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Bottlebrush buckeyeAesculus parviflora | 369 lbf* | 24.3 lb/ft³ |
| California buckeyeAesculus californica | 369 lbf* | 24.3 lb/ft³ |
| Horse chestnutAesculus hippocastanum | 369 lbf* | 24.3 lb/ft³ |
| Ohio buckeyeAesculus glabra | 369 lbf* | 24.3 lb/ft³ |
| Painted buckeyeAesculus sylvatica | 369 lbf* | 24.3 lb/ft³ |
| Red buckeyeAesculus pavia | 369 lbf* | 24.3 lb/ft³ |
| Yellow buckeyeAesculus flava | 369 lbf* | 24.3 lb/ft³ |