genus
Albizia
Woods sold under several trade names often come from one genus. These 11 share the genus Albizia, so they are close relatives and frequent substitutes for each other.
3 of 11 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AlbizziaAlbizia spp. | 955 lbf | 40.0 lb/ft³ |
| BataiAlbizia falcataria | 344 lbf* | 24.0 lb/ft³ |
| Chinese albiziaAlbizia chinensis | 608 lbf* | 30.7 lb/ft³ |
| Inga-de-porcoAlbizia pedicellaris = Macrosamanea pedicellaris | 955 lbf | 38.1 lb/ft³ |
| KokkoAlbizia lebbek | 1,240 lbf | 39.0 lb/ft³ |
| MimosaAlbizia julibrissin | 875 lbf* | 36.3 lb/ft³ |
| Naked albiziaAlbizia carbonaria | 1,007 lbf* | 38.8 lb/ft³ |
| Tall albiziaAlbizia procera | 1,538 lbf* | 47.3 lb/ft³ |
| Ukall ra ngebardAlbizia retusa | 1,103 lbf* | 40.5 lb/ft³ |
| Whiteflower albiziaAlbizia saponaria | 1,309 lbf* | 43.8 lb/ft³ |
| Woman's tongueAlbizia lebbeck | 1,363 lbf* | 44.7 lb/ft³ |