Wood Record

genus

Alnus

Woods sold under several trade names often come from one genus. These 9 share the genus Alnus, so they are close relatives and frequent substitutes for each other.

1 of 9 carry a published Janka test.

WoodJankaDensity
Arizona alderAlnus oblongifolia479 lbf*27.5 lb/ft³
European alderAlnus glutinosa479 lbf*27.5 lb/ft³
Gray alderAlnus incana479 lbf*27.5 lb/ft³
Green alderAlnus viridis479 lbf*27.5 lb/ft³
Hazel alderAlnus serrulata479 lbf*27.5 lb/ft³
Italian alderAlnus cordata479 lbf*27.5 lb/ft³
Nepal alderAlnus nepalensis608 lbf*30.7 lb/ft³
Red alderAlnus rubra590 lbf28.7 lb/ft³
White alderAlnus rhombifolia479 lbf*27.5 lb/ft³