genus
Amelanchier
Woods sold under several trade names often come from one genus. These 3 share the genus Amelanchier, so they are close relatives and frequent substitutes for each other.
0 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Allegheny serviceberryAmelanchier laevis | 1,852 lbf* | 51.5 lb/ft³ |
| Common serviceberryAmelanchier arborea | 1,852 lbf* | 51.5 lb/ft³ |
| Roundleaf serviceberryAmelanchier sanguinea | 1,852 lbf* | 51.5 lb/ft³ |