Wood Record

genus

Anacardium

Woods sold under several trade names often come from one genus. These 5 share the genus Anacardium, so they are close relatives and frequent substitutes for each other.

5 of 5 carry a published Janka test.

WoodJankaDensity
CajuaçuAnacardium giganteum505 lbf30.6 lb/ft³
CajuaçuAnacardium occidentale = Anacardium microcarpum591 lbf28.7 lb/ft³
CajuaçuAnacardium parvifolium657 lbf31.5 lb/ft³
CajuaçuAnacardium spruceanum560 lbf31.5 lb/ft³
EspaveAnacardium excelsum470 lbf30.0 lb/ft³