genus
Annona
Woods sold under several trade names often come from one genus. These 7 share the genus Annona, so they are close relatives and frequent substitutes for each other.
1 of 7 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Annona cherimolaAnnona cherimola | 1,255 lbf* | 43.0 lb/ft³ |
| Custard appleAnnona reticulata | 791 lbf* | 34.7 lb/ft³ |
| EmbiraAnnona exsucca = Rollinia exsucca | 864 lbf | 39.6 lb/ft³ |
| Mountain soursopAnnona montana | 753 lbf* | 33.9 lb/ft³ |
| Pond-appleAnnona glabra | 753 lbf* | 33.9 lb/ft³ |
| SoursopAnnona muricata | 479 lbf* | 27.5 lb/ft³ |
| Sugar appleAnnona squamosa | 1,419 lbf* | 45.5 lb/ft³ |