Woods sold under several trade names often come from one genus. These 5 share the genus Araucaria, so they are close relatives and frequent substitutes for each other.

1 of 5 carry a published Janka test.

WoodJankaDensity
Hoop-PineAraucaria spp.576 lbf*31.0 lb/ft³
Monkeypuzzle treeAraucaria araucana766 lbf*38.0 lb/ft³
New Caledonia pineAraucaria columnaris554 lbf*30.7 lb/ft³
Parana pineAraucaria angustifolia645 lbf*33.9 lb/ft³
Parana-pineAraucaria augustifolia780 lbf34.7 lb/ft³