genus
Arbutus
Woods sold under several trade names often come from one genus. These 4 share the genus Arbutus, so they are close relatives and frequent substitutes for each other.
0 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Arizona madroneArbutus arizonica | 1,363 lbf* | 44.7 lb/ft³ |
| Pacific madroneArbutus menziesii | 1,363 lbf* | 44.7 lb/ft³ |
| Strawberry treeArbutus unedo | 1,363 lbf* | 44.7 lb/ft³ |
| Texas madroneArbutus xalapensis | 1,363 lbf* | 44.7 lb/ft³ |