Wood Record

genus

Artocarpus

Woods sold under several trade names often come from one genus. These 4 share the genus Artocarpus, so they are close relatives and frequent substitutes for each other.

1 of 4 carry a published Janka test.

WoodJankaDensity
Artocarpus heterophyllusArtocarpus heterophyllus875 lbf*36.3 lb/ft³
BreadfruitArtocarpus altilis451 lbf*26.7 lb/ft³
KeledangArtocarpus spp.1,250 lbf44.0 lb/ft³
MarangArtocarpus odoratissimus1,152 lbf*41.3 lb/ft³