genus
Aspidosperma
Woods sold under several trade names often come from one genus. These 3 share the genus Aspidosperma, so they are close relatives and frequent substitutes for each other.
3 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AraracangaAspidosperma desmanthum | 1,757 lbf | 51.2 lb/ft³ |
| PerobaAspidosperma macrocarpon | 1,852 lbf | 48.7 lb/ft³ |
| Peroba rosaAspidosperma spp., peroba group | 1,730 lbf | 51.5 lb/ft³ |