genus
Astronium
Woods sold under several trade names often come from one genus. These 3 share the genus Astronium, so they are close relatives and frequent substitutes for each other.
3 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Goncalo alvesAstronium graveolens | 2,160 lbf | 67.7 lb/ft³ |
| MuiracatiaraAstronium ulei | 1,684 lbf | 55.9 lb/ft³ |
| Muiracatiara-rajadaAstronium lecointei | 2,051 lbf | 61.3 lb/ft³ |