Woods sold under several trade names often come from one genus. These 3 share the genus Avicennia, so they are close relatives and frequent substitutes for each other.

0 of 3 carry a published Janka test.

WoodJankaDensity
Avicennia marinaAvicennia marina1,658 lbf*48.9 lb/ft³
BiutAvicennia alba1,725 lbf*49.9 lb/ft³
Black mangroveAvicennia germinans2,139 lbf*55.1 lb/ft³