Woods sold under several trade names often come from one genus. These 6 share the genus Bauhinia, so they are close relatives and frequent substitutes for each other.

0 of 6 carry a published Janka test.

WoodJankaDensity
Butterfly treeBauhinia purpurea1,103 lbf*40.5 lb/ft³
Mountain ebonyBauhinia variegata1,255 lbf*43.0 lb/ft³
Napoleon's plumeBauhinia monandra1,309 lbf*43.8 lb/ft³
Petite flamboyant bauhiniaBauhinia multinervia2,139 lbf*55.1 lb/ft³
St. Thomas treeBauhinia tomentosa2,692 lbf*61.3 lb/ft³
TexasplumeBauhinia lunarioides2,058 lbf*54.1 lb/ft³