Wood Record

genus

Betula

Woods sold under several trade names often come from one genus. These 12 share the genus Betula, so they are close relatives and frequent substitutes for each other.

3 of 12 carry a published Janka test.

WoodJankaDensity
Alaska paper birchBetula neoalaskana——
Asian white birchBetula platyphylla1,007 lbf*38.8 lb/ft³
Downy birchBetula pubescens1,007 lbf*38.8 lb/ft³
Gray birchBetula populifolia753 lbf*33.9 lb/ft³
Himalayan birchBetula utilis1,007 lbf*38.8 lb/ft³
Paper birchBetula papyrifera910 lbf38.5 lb/ft³
River birchBetula nigra915 lbf*37.1 lb/ft³
Silver birchBetula pendula1,203 lbf*42.1 lb/ft³
Sweet birchBetula lenta1,470 lbf45.4 lb/ft³
Virginia roundleaf birchBetula uber1,007 lbf*38.8 lb/ft³
Water birchBetula occidentalis1,007 lbf*38.8 lb/ft³
Yellow birchBetula alleghaniensis1,260 lbf43.3 lb/ft³