Woods sold under several trade names often come from one genus. These 2 share the genus Bixa, so they are close relatives and frequent substitutes for each other.

1 of 2 carry a published Janka test.

WoodJankaDensity
LipsticktreeBixa orellana423 lbf*26.0 lb/ft³
Urucu-da-mataBixa arborea437 lbf23.5 lb/ft³