Wood Record

genus

Brosimum

Woods sold under several trade names often come from one genus. These 10 share the genus Brosimum, so they are close relatives and frequent substitutes for each other.

10 of 10 carry a published Janka test.

WoodJankaDensity
Amapá-doceBrosimum parinarioides1,250 lbf43.8 lb/ft³
Amapá-doceBrosimum potabile1,184 lbf40.5 lb/ft³
CapomoBrosimum spp. (Alicastrum group)1,340 lbf49.4 lb/ft³
Conduru / pau-vermelhoBrosimum rubescens2,062 lbf50.6 lb/ft³
GarroteBrosimum sp1,074 lbf36.2 lb/ft³
JanitáBrosimum alicastrum2,059 lbf58.7 lb/ft³
Janitá / garroteBrosimum utile946 lbf36.2 lb/ft³
MururéBrosimum gaudichaudii3,036 lbf56.8 lb/ft³
MururéBrosimum acutifolium subsp interjectum1,120 lbf42.1 lb/ft³
SandeBrosimum spp., utile group900 lbf37.1 lb/ft³