genus
Buchenavia
Woods sold under several trade names often come from one genus. These 5 share the genus Buchenavia, so they are close relatives and frequent substitutes for each other.
5 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| CuiaranaBuchenavia grandis | 2,513 lbf | 55.6 lb/ft³ |
| TanibocaBuchenavia cf viridiflora | 2,191 lbf | 54.9 lb/ft³ |
| TanimbucaBuchenavia sp | 2,829 lbf | 53.7 lb/ft³ |
| TanimbucaBuchenavia tetraphylla = Buchenavia capitata | 1,640 lbf | 52.4 lb/ft³ |
| Yellow SandersBuchenavia capitata | 1,220 lbf | 47.0 lb/ft³ |