Wood Record

genus

Byrsonima

Woods sold under several trade names often come from one genus. These 4 share the genus Byrsonima, so they are close relatives and frequent substitutes for each other.

0 of 4 carry a published Janka test.

WoodJankaDensity
DoncellaByrsonima spicata1,419 lbf*45.5 lb/ft³
Long Key locustberryByrsonima lucida1,203 lbf*42.1 lb/ft³
Maricao cimunByrsonima crassifolia1,475 lbf*46.4 lb/ft³
SerretteByrsonima coriacea var. spicata1,538 lbf*46.0 lb/ft³