genus
Calophyllum
Woods sold under several trade names often come from one genus. These 4 share the genus Calophyllum, so they are close relatives and frequent substitutes for each other.
2 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Alexandrian laurelCalophyllum inophyllum | 1,255 lbf* | 43.0 lb/ft³ |
| BintangorCalophyllum spp. | 1,475 lbf | 40.0 lb/ft³ |
| OlebtachesCalophyllum soulattri | 1,054 lbf* | 39.6 lb/ft³ |