genus
Campnosperma
Woods sold under several trade names often come from one genus. These 2 share the genus Campnosperma, so they are close relatives and frequent substitutes for each other.
1 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| KelelacharmCampnosperma brevipetiolatum | 423 lbf* | 26.0 lb/ft³ |
| SajoCampnosperma panamensis | 425 lbf | 25.0 lb/ft³ |