genus
Canarium
Woods sold under several trade names often come from one genus. These 6 share the genus Canarium, so they are close relatives and frequent substitutes for each other.
1 of 6 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| African CanaríumCanarium schweinfurthii | 670 lbf | 30.0 lb/ft³ |
| Canarium vulgareCanarium vulgare | 875 lbf* | 36.3 lb/ft³ |
| KedondongCanarium spp. | 695 lbf* | 33.0 lb/ft³ |
| LukerrCanarium indicum | 1,103 lbf* | 40.5 lb/ft³ |
| MaaliCanarium vitiense | 915 lbf* | 37.1 lb/ft³ |
| MesecheuesCanarium hirsutum | 960 lbf* | 38.0 lb/ft³ |