Woods sold under several trade names often come from one genus. These 2 share the genus Cariniana, so they are close relatives and frequent substitutes for each other.

2 of 2 carry a published Janka test.

WoodJankaDensity
AlbarcoCariniana spp.1,020 lbf35.0 lb/ft³
Tauari-vermelhoCariniana micrantha970 lbf42.5 lb/ft³