genus
Carpinus
Woods sold under several trade names often come from one genus. These 3 share the genus Carpinus, so they are close relatives and frequent substitutes for each other.
0 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| American hornbeamCarpinus caroliniana | 1,363 lbf* | 44.7 lb/ft³ |
| European hornbeamCarpinus betulus | 1,658 lbf* | 48.9 lb/ft³ |
| Japanese hornbeamCarpinus japonica | 1,309 lbf* | 43.8 lb/ft³ |