genus
Carya
Woods sold under several trade names often come from one genus. These 13 share the genus Carya, so they are close relatives and frequent substitutes for each other.
5 of 13 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Bitternut hickoryCarya cordiformis | 1,461 lbf* | 46.1 lb/ft³ |
| Black hickoryCarya texana | 1,598 lbf* | 48.1 lb/ft³ |
| Mockernut hickoryCarya alba | 1,970 lbf | 50.3 lb/ft³ |
| Nutmeg hickoryCarya myristiciformis | 1,190 lbf* | 42.0 lb/ft³ |
| Pecan hickoryCarya illinoinensis | 1,820 lbf | 46.1 lb/ft³ |
| Pignut hickoryCarya glabra | 2,140 lbf | 52.4 lb/ft³ |
| Red hickoryCarya ovalis | 1,598 lbf* | 48.1 lb/ft³ |
| Sand hickoryCarya pallida | 1,598 lbf* | 48.1 lb/ft³ |
| Scrub hickoryCarya floridana | 1,598 lbf* | 48.1 lb/ft³ |
| Shagbark hickoryCarya ovata | 1,880 lbf | 50.3 lb/ft³ |
| Shellbark hickoryCarya laciniosa | 1,810 lbf | 48.3 lb/ft³ |
| Southern shagbark hickoryCarya carolinae-septentrionalis | 1,598 lbf* | 48.1 lb/ft³ |
| Water hickoryCarya aquatica | 1,277 lbf* | 43.3 lb/ft³ |