genus
Caryocar
Woods sold under several trade names often come from one genus. These 3 share the genus Caryocar, so they are close relatives and frequent substitutes for each other.
3 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| PequiáCaryocar villosum | 1,133 lbf | 48.7 lb/ft³ |
| PequiaranaCaryocar glabrum | 1,642 lbf | 48.7 lb/ft³ |
| PiquiaCaryocar spp. | 1,720 lbf | 54.0 lb/ft³ |