genus

Casearia

Woods sold under several trade names often come from one genus. These 6 share the genus Casearia, so they are close relatives and frequent substitutes for each other.

1 of 6 carry a published Janka test.

WoodJankaDensity
CrackopenCasearia sylvestris1,598 lbf*48.1 lb/ft³
Gia verdeCasearia arborea1,475 lbf*46.4 lb/ft³
Guyanese wild coffeeCasearia guianensis1,990 lbf*53.3 lb/ft³
MuirungiCasearia battiscombei720 lbf40.0 lb/ft³
Rabo de rantonCasearia aculeata1,725 lbf*49.9 lb/ft³
Wild honeytreeCasearia decandra1,788 lbf*50.7 lb/ft³