1 of 4 carry a published Janka test.

WoodJankaDensity
Apple blossomCassia javanica1,725 lbf*49.9 lb/ft³
CanafístulaCassia fastuosa2,500 lbf54.3 lb/ft³
Golden showerCassia fistula2,139 lbf*55.1 lb/ft³
Pink showerCassia grandis1,852 lbf*51.5 lb/ft³