Wood Record

genus

Cassipourea

Woods sold under several trade names often come from one genus. These 2 share the genus Cassipourea, so they are close relatives and frequent substitutes for each other.

1 of 2 carry a published Janka test.

WoodJankaDensity
GoatwoodCassipourea guianensis2,210 lbf*55.9 lb/ft³
PillarwoodCassipourea malosana1,450 lbf47.0 lb/ft³