Castanea
Woods sold under several trade names often come from one genus. These 5 share the genus Castanea, so they are close relatives and frequent substitutes for each other.
1 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Allegheny chinkapinCastanea pumila | 573 lbf* | 29.8 lb/ft³ |
| American chestnutCastanea dentata | 540 lbf | 30.1 lb/ft³ |
| Chinese chestnutCastanea mollissima | 573 lbf* | 29.8 lb/ft³ |
| Japanese chestnutCastanea crenata | 573 lbf* | 29.8 lb/ft³ |
| Sweet chestnutCastanea sativa | 1,103 lbf* | 40.5 lb/ft³ |