genus
Castilla
Woods sold under several trade names often come from one genus. These 2 share the genus Castilla, so they are close relatives and frequent substitutes for each other.
1 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| CauchoCastilla ulei | 313 lbf | 29.3 lb/ft³ |
| Panama rubbertreeCastilla elastica | 423 lbf* | 26.0 lb/ft³ |