Wood Record

genus

Casuarina

Woods sold under several trade names often come from one genus. These 4 share the genus Casuarina, so they are close relatives and frequent substitutes for each other.

1 of 4 carry a published Janka test.

WoodJankaDensity
Beach sheoakCasuarina equisetifolia3,241 lbf*66.9 lb/ft³
CasuarinaCasuarina spp.3,200 lbf64.0 lb/ft³
Gray sheoakCasuarina glauca2,448 lbf*58.7 lb/ft³
River sheoakCasuarina cunninghamiana1,990 lbf*53.3 lb/ft³