| Wood | Janka | Density |
|---|---|---|
| Chinese catalpaCatalpa ovata | 509 lbf* | 28.2 lb/ft³ |
| Haitian catalpaCatalpa longissima | 1,007 lbf* | 38.8 lb/ft³ |
| Northern catalpaCatalpa speciosa | 509 lbf* | 28.2 lb/ft³ |
| Southern catalpaCatalpa bignonioides | 509 lbf* | 28.2 lb/ft³ |