genus
Cedrela
Woods sold under several trade names often come from one genus. These 3 share the genus Cedrela, so they are close relatives and frequent substitutes for each other.
3 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| CedroCedrela odorata | 1,373 lbf | 29.3 lb/ft³ |
| Spanish-cedarCedrela spp. | 600 lbf | 35.0 lb/ft³ |
| ToonCedrela spp. (mainly C toona) | 550 lbf | 31.5 lb/ft³ |