Wood Record

genus

Cedrelinga

Woods sold under several trade names often come from one genus. These 2 share the genus Cedrelinga, so they are close relatives and frequent substitutes for each other.

1 of 2 carry a published Janka test.

WoodJankaDensity
Cedro-RanaCedrelinga catenaeformis1,103 lbf*40.5 lb/ft³
TornilloCedrelinga cateniformis787 lbf35.0 lb/ft³