0 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Atlas cedarCedrus atlantica | 554 lbf* | 30.7 lb/ft³ |
| Cedar of LebanonCedrus libani | 692 lbf* | 35.5 lb/ft³ |
| Deodar cedarCedrus deodara | 844 lbf* | 40.5 lb/ft³ |