genus
Celtis
Woods sold under several trade names often come from one genus. These 5 share the genus Celtis, so they are close relatives and frequent substitutes for each other.
2 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| African CeltisCeltis spp. | 1,670 lbf | 45.0 lb/ft³ |
| Celtis paniculataCeltis paniculata | 1,309 lbf* | 43.8 lb/ft³ |
| Chinese hackberryCeltis sinensis | 915 lbf* | 37.1 lb/ft³ |
| HackberryCeltis occidentalis | 880 lbf | 37.1 lb/ft³ |
| SugarberryCeltis laevigata | 915 lbf* | 37.1 lb/ft³ |