Wood Record

genus

Chamaecyparis

Woods sold under several trade names often come from one genus. These 5 share the genus Chamaecyparis, so they are close relatives and frequent substitutes for each other.

3 of 5 carry a published Janka test.

WoodJankaDensity
Atlantic white cedarChamaecyparis thyoides350 lbf22.3 lb/ft³
HinokiChamaecyparis obtusa599 lbf*32.3 lb/ft³
Port-Orford cedarChamaecyparis lawsoniana630 lbf30.1 lb/ft³
Sawara-cypressChamaecyparis pisifera469 lbf*27.5 lb/ft³
Yellow cedarChamaecyparis nootkatensis580 lbf30.8 lb/ft³