Woods sold under several trade names often come from one genus. These 3 share the genus Chionanthus, so they are close relatives and frequent substitutes for each other.
0 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| BridgotreeChionanthus compactus | 4,196 lbf* | 75.4 lb/ft³ |
| Chinese fringetreeChionanthus retusus | 1,923 lbf* | 52.4 lb/ft³ |
| White rosewoodChionanthus domingensis | 2,963 lbf* | 64.1 lb/ft³ |