genus
Chrysophyllum
Woods sold under several trade names often come from one genus. These 5 share the genus Chrysophyllum, so they are close relatives and frequent substitutes for each other.
2 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Bastard redwoodChrysophyllum argenteum | 2,692 lbf* | 61.3 lb/ft³ |
| GoiabãoChrysophyllum lucentifolium = Pouteria pachycarpa | 2,646 lbf | 58.1 lb/ft³ |
| MaçarandubaranaChrysophyllum prieurii | 2,725 lbf | 61.8 lb/ft³ |
| SatinleafChrysophyllum oliviforme | 2,607 lbf* | 60.4 lb/ft³ |
| Star appleChrysophyllum cainito | 2,448 lbf* | 58.7 lb/ft³ |