Wood Record

genus

Cinnamomum

Woods sold under several trade names often come from one genus. These 4 share the genus Cinnamomum, so they are close relatives and frequent substitutes for each other.

0 of 4 carry a published Janka test.

WoodJankaDensity
CamphortreeCinnamomum camphora875 lbf*36.3 lb/ft³
CassiaCinnamomum aromaticum915 lbf*37.1 lb/ft³
CinnamonCinnamomum verum1,054 lbf*39.6 lb/ft³
Cinnamon WoodCinnamomum spp.660 lbf*32.0 lb/ft³